材質 |
化學成份 Chemical Composition (%) |
最高工作溫度MAX WORK TEMP |
特殊性 | |||||
C |
Si |
Mn |
Ni |
Cr |
Mo | |||
A3 |
≤0.22 |
≤0.3 |
≤0.65 |
- |
- |
- |
400° |
普通網帶 |
45# |
≤0.50 |
≤0.37 |
≤0.80 |
≤0.25 |
≤0.25 |
|
500° |
普通網帶 |
1cr13 |
≤0.15 |
≤0.6 |
≤0.6 |
- |
12-14 |
- |
650 ° |
普通網帶 |
1cr17 |
≤0.15 |
≤0.6 |
≤0.6 |
- |
12-18 |
- |
650 ° |
普通網帶 |
304M |
≤0.06 |
≤1.0 |
≤2.0 |
8.9-10.0 |
18-20 |
- |
750° |
普通網帶 |
304L |
≤0.03 |
≤1.0 |
≤2.0 |
9-13 |
18-20 |
- |
750 ° |
耐晶界腐蝕 |
316 |
≤0.08 |
≤1.0 |
≤2.0 |
10-14 |
16-18 |
2-3 |
750° |
耐腐蝕 |
316L |
≤0.03 |
≤1.0 |
≤2.0 |
12-15 |
16-18 |
2-3 |
750° |
耐晶界腐蝕 |
309S |
≤0.08 |
≤1.0 |
≤2.0 |
12-15 |
22-24 |
- |
950 ° |
耐長時間高溫 |
310S |
≤0.08 |
≤1.5 |
≤2.0 |
19-22 |
24-26 |
- |
(國產)1000 ° |
耐高溫及高溫拉伸 |
314 |
≤0.25 |
≤1.5-3.0 |
≤2.0 |
19-22 |
23-26 |
- |
(國產)1050 ° |
在310基礎上提高抗氧性 |
CI20NI80 |
≤0.15 |
≤0.4-1.3 |
≤0.7 |
75-78 |
20-23 |
- |
1200 ° |
耐高溫、抗氧化 |